Thermal Deviation
Thermal processes that involve the melting and cooling of solder can induce permanent mechanical changes in the shape of printed circuit boards and their components. When surface mount reflow distortion occurs, the mismatch in thermal expansion between layers causes the board to bow. This movement can pull solder balls away from their pads.
Warpage Quantification
Optical inspection systems measure the magnitude of the displacement at the peak temperature of the oven. Managing surface mount reflow distortion requires careful control of the heating rate and the temperature of the cooling zones. It is quantified in microns per millimeter of length.
Substrate Influence
The glass transition temperature of the epoxy resin determines the stiffness of the board during the soldering cycle. High Tg materials are less prone to surface mount reflow distortion because they maintain their structural integrity at higher temperatures. Balancing the copper distribution on each layer also reduces the tendency to warp.
Designers use this information to select prepreg materials with suitable glass transition points.
Interconnect Failure
Excessive movement leads to non wet opens or head in pillow defects in high density packages. Analyzing surface mount reflow distortion helps in optimizing the stencil design to ensure sufficient solder paste remains in contact with the component leads.