Laminate Deficiency
Physical condition where an insufficient volume of resin exists to completely fill the gaps between the glass fibers and the copper features in a pcb. Identifying resin starvation involves locating voids or dry spots within the dielectric layers of the finished board. The presence of this defect typically occurs during the lamination process if the resin flow is restricted or if the material volume is inadequate for the design.
Void Formation
Lack of material creates air pockets that compromise the electrical insulation. Instances of resin starvation are often found in areas with high copper density where the resin cannot flow easily.
Failure Mechanism
Entrapped air in a region of resin starvation can lead to catastrophic delamination when the board is exposed to the high temperatures of solder reflow. These voids also act as pathways for moisture absorption and conductive anodic filament growth. Inspection for this defect involves micro-sectioning and optical microscopy to identify areas where the glass weave is not fully encapsulated.
Prevention Strategy
Correcting the resin volume in the prepreg selection prevents the occurrence of dry spots in high-density designs. Adjusting the lamination press parameters to control the rate of resin flow also helps ensure complete wet-out of the glass fibers. Heavily etched layers require more resin to fill the large copper-free areas compared to dense signal layers.
Reliable manufacturing depends on matching the resin content of the prepreg to the specific copper topography of the internal layers.