Internal Tension
An internal mechanical force is established within a thin layer of material deposited onto a thicker substrate due to thermal or structural mismatches. This force, known as thin film stress, exists in all deposited metals, oxides, and nitrides on a silicon wafer. The boundary of this effect is the limit where the film delaminates from the substrate or causes the wafer to fracture.
Manufacturing Control
The thermal expansion difference between the film and the silicon substrate is a major cause of thin film stress when the wafer cools from the deposition temperature. Intrinsic forces also develop during the deposition process as atoms are arranged in non-equilibrium positions. By adjusting parameters such as deposition temperature, sputtering power, and gas flow rates, manufacturers can minimize this force.
Structural Response
Suspended microstructures like cantilevers or membranes will warp or curl if there is a stress gradient through the thickness of the film. This warping alters the distance between capacitor plates, which changes the baseline capacitance and shifts the sensor out of its calibrated range. In severe cases, high thin film stress can cause the structure to break during the release etch process.
Metrological Verification
Process monitors measure the change in wafer curvature to calculate the average stress of the deposited film.