Assembly Expansion
Physical deformation generated within electronic components and circuit boards during the high temperature soldering process. If reflow thermal strain occurs as materials with different coefficients of thermal expansion grow at different rates, the temperature rise can cause warping of the substrate or the cracking of sensitive ceramic capacitors.
Solder Fatigue
The mismatch between the expansion of the component body and the board places a mechanical load on the solder connections as they solidify. High levels of reflow thermal strain can lead to residual stresses that weaken the joint before the product leaves the factory. Managing this strain requires a carefully controlled temperature profile that includes a gradual preheat and a limited time above the liquidus point.
Expansion Coefficient
Low expansion laminates reduce the total movement during the heating cycle.
Warp Control
Large integrated circuits are particularly susceptible to this issue because their surface area amplifies the total amount of physical shift. Monitoring reflow thermal strain involves using moire interferometry or shadow moire to map the flatness of the board in real time inside the oven. These measurements help engineers adjust the support structures and the oven zones to keep the assembly within its elastic limit.
Failure to manage these forces results in lifted leads and intermittent connections that are difficult to diagnose.