Hermetic Interconnect
A rigid structural sub-assembly consisting of metallic conductor pins secured within a metallic outer frame by fused inorganic glass preforms provides a robust, gas-tight electrical passthrough. In pressure transducers, vacuum chambers and microelectronic sensor enclosures, the glass-to-metal header maintains hermetic isolation while transferring electrical signals across harsh environmental boundaries. Fused glass acts simultaneously as a structural insulator and an impervious hermetic seal between individual terminal pins and the surrounding outer metal body.
Matched seals balance thermal expansion coefficients between glass and kovar alloys, while compression seals rely on outer steel bodies shrinking around glass during cooling. The assembly ceases to provide hermeticity if thermal or mechanical shock cracks the vitreous glass matrices.
Sealing Mechanics
High-temperature furnace firing melts the glass preform at temperatures exceeding eight hundred degrees Celsius, wetting surrounding metal oxide surfaces to establish dense interfacial bonds. Compression assemblies exploit the higher thermal expansion rate of outer stainless steel barrels relative to internal borosilicate glass, generating continuous radial compressive stress against the glass core upon cooldown. Pin conductors pass straight through these insulating beads, maintaining electrical isolation while resisting outward mechanical expulsion under internal pressure.
Meniscus control agents optimize wetting geometry to avoid stress concentration notches at pin exit points.
Failure Modes
Exposure to mechanical bending moments, excessive torque during installation or rapid temperature cycling initiates radial micro-fissuring inside the brittle glass insulator. Chemical attack from hydrofluoric acid or concentrated hot alkaline media leaches silicate networks, eroding insulation resistance and degrading structural hermeticity. If conductor pins suffer severe lateral deflection during handling, interfacial glass-to-metal shear bonds fracture, opening microscopic leak paths.
Atmospheric moisture then penetrates the cracked matrix, initiating electrolytic pin corrosion and causing elevated dielectric surface leakage.
Leak Qualification
Hermetic qualification mandates continuous verification via helium mass spectrometer leak testing performed in accordance with standardized MIL-STD-883 or equivalent industrial test procedures. Vacuum gross and fine leak testing sets allowable limits, rejecting headers displaying tracer gas leakage rates exceeding ten to the power of negative eight standard atmospheric cubic centimeters per second. Dielectric withstanding voltage tests confirm that internal glass insulators resist electrical breakdown under high voltage potentials applied across terminal pins and the metal body.
Solderability and pin pull-strength testing verify that downstream wire bonding or lead soldering operations will not fracture brittle glass seals.