Reliability Assessment
Predictive formulas estimate the time to failure for electronic components exposed to humidity and heat. The peck model expands the Arrhenius equation by including a power-law term for relative humidity. This combination shows how moisture speeds up corrosion and other chemical degradation processes in non-hermetic packages.
Stress Factor
Environmental variables such as vapor pressure and temperature determine the acceleration of the wear-out phase. Within the peck model, the humidity exponent typically ranges between two and three for most epoxy-encapsulated semiconductors. Higher values indicate a greater sensitivity to moisture ingress at the interface between the lead frame and the plastic.
Test Acceleration
Laboratory conditions use high pressure and temperature to compress years of field exposure into a few hundred hours. The peck model provides the mathematical basis for highly accelerated stress testing where the atmosphere is saturated with water vapor. These results allow for the qualification of new packaging materials and assembly processes before the start of volume production.
Constraint Boundary
Validity of the prediction assumes that the failure mode remains the same at both high and low stress levels. The peck model does not account for condensation or liquid water contact on the surface of the die. Testing must be conducted below the maximum rated storage temperature.