Barrier Layer
Diffusion barrier layers are deposited between a copper substrate and an outer gold or tin plating to prevent interdiffusion and solder joint degradation. This intermediate deposit, referred to as a nickel underplate, is a critical layer in the leadframe metallization stack.
Diffusion Blocker
Copper atoms tend to migrate rapidly into tin or gold coatings at elevated temperatures. The nickel underplate acts as an effective physical barrier because the diffusion rates of copper and tin through nickel are extremely low. This blocking action prevents the formation of weak copper-tin intermetallic compounds on the surface.
Interface Strength
Solder joints formed on a nickel surface display excellent mechanical properties due to the controlled growth of nickel-tin intermetallics. Unlike copper-tin phases, the nickel-tin reaction is slow and uniform, resulting in a thin and stable interface. This stability ensures that the joint remains mechanically sound under thermal and mechanical stress.
Excessive thickness of the nickel must be avoided to prevent plating peel or cracking due to high internal stress.
Deposition Standard
Quality specifications define the minimum required nickel thickness to guarantee barrier effectiveness over the component lifetime. Thicknesses are measured using X-ray fluorescence during the electroplating process. These values are recorded on the certificate of conformance.