Barrier Performance
Material permeation metrics evaluate the quantity of oxygen gas that passes through a unit area of a plastic film or barrier over a specific duration under steady conditions. The oxygen transmission rate is the standard measurement used to define the barrier efficacy of packaging films and protective coatings. This parameter is necessary for determining how well a material can prevent the entry of oxygen into sensitive packages.
It is expressed in cubic centimeters per square meter over a twenty four hour period.
Transport Process
The transfer process involves three stages, starting with the adsorption of gas molecules onto the high concentration side of the barrier. These molecules then diffuse through the polymer bulk, driven by the concentration gradient across the material thickness. Finally, they desorb from the low concentration surface into the surrounding atmosphere or carrier gas.
This continuous pathway is highly dependent on both the solubility of the gas and its diffusion coefficient within the material.
Influence Factor
Environmental temperature and relative humidity can severely degrade the barrier performance of polymer films, leading to an increase in this transmission parameter. For hydrophilic polymers such as ethylene vinyl alcohol, high humidity causes water molecules to plasticize the material, which drastically increases the oxygen transmission rate. This effect requires food and pharmaceutical packaging designs to incorporate protective hydrophobic layers to shield the primary gas barrier from moisture in the environment.
Test Methodology
Standard testing is performed using a diffusion cell where a film specimen is clamped between two chambers. One chamber is purged with carrier gas, while the other receives oxygen. A coulometric sensor then measures the quantity of gas that permeates through the film.