Corrosion Testing
Environmental testing standards specify the conditions for subjecting electronic components to a controlled salt spray environment. The standard designated JESD22 B117A defines the apparatus and procedure required to execute an accelerated corrosion evaluation. This document ensures that the resistance of protective coatings, surface finishes, and metallic joints to salt-induced degradation is measured consistently.
Chamber Control
Elevated temperature and continuous atomization of a sodium chloride solution simulate harsh marine or coastal environments inside the exposure enclosure. During the JESD22 B117A test, the chamber temperature is maintained at thirty-five degrees Celsius while a five percent salt solution is continuously sprayed. This creates a corrosive mist that accelerates the degradation of any exposed metal surfaces on the test boards.
This controlled exposure is critical for predicting the long-term reliability of electronic assemblies destined for outdoor or industrial use.
Specimen Positioning
Orientation of the test specimens inside the chamber must prevent the accumulation of large droplets on critical surfaces. Under JESD22 B117A, the boards are held at a specific angle from the vertical to allow the salt mist to flow freely across the test surfaces.
Post-Exposure Evaluation
Visual inspection and electrical testing of the specimens are conducted after the salt exposure is complete. This post-test phase measures changes in contact resistance or identifies the formation of corrosion products that could cause electrical shorts.