Crystal Impurity
Atomic impurities residing at non-lattice positions within a silicon crystal lattice influence the mechanical and electrical properties of the semiconductor material. The presence of interstitial oxygen typically occurs during the Czochralski growth process when the molten silicon interacts with the quartz crucible.
Gettering Mechanism
Controlled precipitation of these atoms creates internal sites that trap mobile metallic contaminants. By managing the level of interstitial oxygen, manufacturers prevent these metals from reaching the active device region where they would cause leakage currents. This internal cleaning improves the reliability of the finished chips.
Structural Strengthening
High concentrations of oxygen atoms increase the yield strength of the wafer and help it resist warping during high-temperature furnace steps. If the amount of interstitial oxygen is too low, the silicon becomes brittle and prone to slip dislocations. Thermal stress during processing can then lead to catastrophic wafer breakage.
Mechanical integrity depends on maintaining this concentration within a narrow window specified by the fab.
Concentration Measurement
Fourier transform infrared spectroscopy determines the density of these atoms by measuring the absorption peak at a specific wavelength. Because interstitial oxygen levels drift during subsequent thermal cycles, the measurement is usually performed on the raw wafer.