Surface Coating
Final stages of printed circuit board fabrication often utilize a multi-layer coating to ensure long-term solderability. Electroless nickel immersion gold consists of a nickel layer followed by a thin deposit of gold applied through a chemical displacement reaction. This finish supports high-density designs due to its flat profile and excellent shelf life.
Deposition Process
Autocatalytic reduction deposits nickel onto the copper substrate to create a diffusion barrier. The electroless nickel immersion gold sequence continues with the immersion of the board into a gold salt solution where gold atoms replace surface nickel atoms. Maintaining the chemical balance of the baths prevents the excessive corrosion of the nickel layer.
Interface Integrity
Quality assessments look for the formation of a continuous intermetallic bond during the soldering process. Excessive phosphorus content in the nickel or a poorly controlled gold bath can lead to the brittle failure known as black pad. Electroless nickel immersion gold requires precise monitoring of the bath temperature and pH to ensure the nickel layer remains receptive.
Periodic testing of the gold concentration prevents the layer from becoming too porous or thick.
Metrological Verification
X-ray fluorescence measurement verifies the thickness of both the nickel and gold layers against the procurement specification. Standard tolerances usually require several micrometers of nickel but only a fraction of a micrometer of gold.